SF-1 Oil-Free Composite Bushing

https://www.linkcnc.net/web/image/product.template/2303/image_1920?unique=5eee4bf

¥ 2.21 2.21 CNY ¥ 2.21

Not Available For Sale

Reference weight: approx. 50 g
  • Size

This combination does not exist.

Prices exclude shipping. Submit your order and we will email you a formal quote.

Returns & refunds
7-day returns · custom products excluded
Shipping cost quoted with your order

Bushings and collars · 11 sizes · 11 options in stock

Bushings, sleeves and shaft collars — plain bearings and axial location. The parameters are listed in order of importance: the one at the top decides the most, and no amount of care further down makes up for getting it wrong.

This page lists 11 options: Size 6x8x12 / 8x10x5 / 8x10x6 / 8x10x8 … 11 total. From ¥2.21.

The parts of this item

The parts of a bush or collar

Figure 1 — A bush needs three numbers: bore × outer diameter × length — bore to the shaft, OD to the hole, length sets the support

What each parameter decides

Every parameter below shows the real range available on this page, and what goes wrong if you pick it wrong. Work through them in this order and you will not go far wrong.

ParameterAvailable hereWhat it decidesIf you get it wrong
Size6x8x12 / 8x10x5 / 8x10x6 / 8x10x8 … 11 totaloverall size and the space it needsit will not fit, or it cannot be fastened down

How to choose, step by step

  1. Style — Open type clamps, shaft collar locates axially, flanged type bolts down.

How the options on this page are distributed

How the 11 options on this page are distributed

Figure 2 — how the 11 options on this page are spread across each parameter: the bars on the left show how many options sit in each band, the panel on the right shows the real range of every parameter and how many steps it has.

Variant quick reference

SizePart no.
10x12x20RL-024-10x12x20
12x14x10RL-024-12x14x10
12x14x15RL-024-12x14x15
6x8x12RL-024-6x8x12
8x10x10RL-024-8x10x10
8x10x12RL-024-8x10x12
8x10x15RL-024-8x10x15
8x10x20RL-024-8x10x20
8x10x5RL-024-8x10x5
8x10x6RL-024-8x10x6
8x10x8RL-024-8x10x8

Reading the part numbers

Part no.Configuration
RL-024-10x12x20Size 10x12x20
RL-024-12x14x10Size 12x14x10
RL-024-12x14x15Size 12x14x15

You can order by part number or by selecting the parameters. The part number is fastest, but it does not always encode every parameter — the selector on this page is the authority.

7 common mistakes

  1. A shaft collar is not a bearing. It locates something axially; it is not a sliding surface and will wear the shaft if used as one.
  2. An open bushing only works when clamped. Unclamped it is a loose ring that rotates and slides.
  3. Bronze bushings need lubrication. Run dry and they pick up on the shaft and seize. Only graphite-impregnated bronze tolerates oil-free running.
  4. Aluminium on steel at speed is a bad pair. Aluminium transfers and galls onto the shaft within minutes.
  5. Check the running clearance. Too tight and it seizes when warm, too loose and the axis has play you cannot adjust out.
  6. Measure before you order. Take the old part off and measure it, or send us a photo with the caliper reading — that beats guessing from a model number every time.
  7. Everything here is in millimetres. Where a size is imperial, convert it: 1" = 25.4 mm, 1/4" = 6.35 mm, 3/32" = 2.38 mm.

When to replace it

You do not replace this until it fails — but "still looks usable" and "still reliable" are two different things. Any one of these and it is time:

  • Bore worn oversize; the shaft rocks in it.
  • Scoring or blackening on the running surface — pickup from the shaft.
  • An open bushing that still rotates or slides after clamping.

Fitting and use

Check before assembly

  • Wipe every mating surface with a lint-free cloth. No chips, no burrs, no old grease. One chip is enough to make a bearing noisy.
  • Measure the fits — shaft, bore, centre height — against nominal. More than 0.02 mm out and you should check whether you have the right part.
  • Check the orientation: the side with the shoulder, step or oil hole has to face the right way. Fitted backwards, it is usually scrap on removal.

Assembly

  • Press if you can; do not hammer. If you must tap, use a brass or nylon drift and put the force on the ring that is being fitted, never through the raceway.
  • For an interference fit, heat to 80–100 °C first (oil bath or hot plate — never an open flame on a bearing). Hot fitting is easier and safer than cold pressing.
  • Tighten fasteners in a diagonal pattern in 2–3 stages. Taking one down fully first distorts the housing and cocks the shaft.

Running in

  • Turn it by hand first. It should be smooth, with no tight spot and no axial play. If there is a tight spot, loosen and reseat — do not run it in.
  • Run it slowly and unloaded for 10–20 minutes, then feel the temperature. A clear rise means too much preload or poor alignment.
  • Re-torque the fasteners after running in, then apply load.

Three things not to do

  • Do not hammer. It brinells the raceway, you cannot see it, and it whines forever afterwards.
  • Do not mix brands or precision classes in a matched pair. The load shares unevenly and the poorer one always fails first.
  • Do not skip lubrication on parts that need it. A few hundred hours dry and it seizes.

Matching parts

  • Set screws and circlips
  • Hardened shaft of the same diameter

Lead time, custom work and shipping

  • Stock sizes: dispatched in 1–2 working days, subject to stock
  • Custom: non-standard sizes, materials and treatments are possible — send quantity and drawing
  • Shipping: from Shenzhen; domestic courier by default, DHL or dedicated line for export
  • Volume: quantity pricing available, contact us for a quote

If you cannot find the size you need, or you are not sure which one fits, send us the problem you are solving — what machine it goes on, the dimensions of the part you have, what it has to achieve — and we will match it.

Home Products OEM & Custom About Us Contact Us Catalog +86 (0755) 23221210